Hits: 350 img
Polydimethylsiloxane chains can be manufactured industrially by the following reaction processes: the mass ratio of main agent to hardener is 10 in common laboratory use: 1. After the mixture is evenly mixed, the bubbles in the mixture float to the surface and burst by vacuuming, and then bake in the oven at 120 degrees for about one hour (different temperature and time parameters will produce PDMS with different hardness).